- Dolomite is broken by crusher-qualified material (30-40mm), sintered by a rotary kiln, and calcined into calcine white.
- The product is then cooled by a cooling machine, ground into powder by a ball mill and pressed into balls by a ball press.
- Once crushed, the material is evenly mixed with ferrosilicon powder (containing 75% silicon) and fluorite powder to create a group. This is then placed in a heat-resistant stainless steel reduction tank and reduced in a reduction furnace at 1200-1250°C and 1.33Pa vacuum degree of vacuum to create crude magnesium. After solvent refining, casting, and surface treatment, the magnesium ingot is obtained.